Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Fusabond® E100 Polymer Modifier

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer DuPont
Trade Name Fusabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Fusabond® E100 Polymer Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DuPont™ Fusabond® E100 is an anhydride modified high density polyethylene, mainly intended for use as a component in a blend with other polymers including polyolefins and polyamides. It is not intended for extrusion in its pure form in typical extrusions or coextrusions. Available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. Fusabond® E100 comply with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlayers in composite packages for food use. This regulation describes adhesives that may be safely used as components of articles intended for use in packaging, transporting or holding food. This regulation requires that either (1) the adhesive is separated from the food by a functional barrier, or (2) the quantity of adhesive which contacts fatty or aqueous foods does not exceed the trace amounts at the seams or edges.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D792, ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 115 °C
239 °F
Freezing Point; ASTM D3418
134 °C
273 °F
ASTM D3418, ISO 3146
Vicat Softening Point 127 °C
261 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F