| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 - 11.0 g/cc | 0.0347 - 0.397 lb/in³ | Average value: 1.26 g/cc Grade Count:92 |
| Water Absorption | 0.700 - 48.0 % | 0.700 - 48.0 % | Average value: 5.72 % Grade Count:60 |
| Moisture Absorption at Equilibrium | 0.300 - 4.50 % | 0.300 - 4.50 % | Average value: 0.996 % Grade Count:55 |
| Water Absorption at Saturation | 0.400 - 1.50 % | 0.400 - 1.50 % | Average value: 0.800 % Grade Count:15 |
| Water Vapor Transmission | 2200 - 25000 g/m²/day <br>@Temperature 38.0 - 38.0 °C |
142 - 1610 g/100 in²/day <br>@Temperature 100 - 100 °F |
Average value: 10200 g/m²/day Grade Count:3 |
| 2200 - 25000 g/m²/day <br>@Thickness 0.0150 - 0.0150 mm |
142 - 1610 g/100 in²/day <br>@Thickness 0.000591 - 0.000591 in |
Average value: 10200 g/m²/day Grade Count:3 | |
| Viscosity Test | 190 cm³/g | 190 cm³/g | Average value: 190 cm³/g Grade Count:5 |
| Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00826 cm/cm Grade Count:36 |
| Linear Mold Shrinkage, Transverse | 0.00600 - 0.0150 cm/cm | 0.00600 - 0.0150 in/in | Average value: 0.0115 cm/cm Grade Count:33 |
| Melt Flow | 4.00 - 20.2 g/10 min | 4.00 - 20.2 g/10 min | Average value: 9.28 g/10 min Grade Count:35 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 72.0 - 83.0 | 72.0 - 83.0 | Average value: 75.4 Grade Count:5 |
| Hardness, Shore D | 22.0 - 72.0 | 22.0 - 72.0 | Average value: 49.1 Grade Count:84 |
| Tensile Strength, Ultimate | 9.00 - 62.0 MPa | 1310 - 8990 psi | Average value: 41.4 MPa Grade Count:56 |
| Tensile Strength, Yield | 1.80 - 34.0 MPa | 261 - 4930 psi | Average value: 14.0 MPa Grade Count:39 |
| Elongation at Break | 1.00 - 1000 % | 1.00 - 1000 % | Average value: 392 % Grade Count:73 |
| Elongation at Yield | 15.0 - 36.0 % | 15.0 - 36.0 % | Average value: 25.1 % Grade Count:18 |
| Modulus of Elasticity | 0.00400 - 4.03 GPa | 0.580 - 585 ksi | Average value: 0.331 GPa Grade Count:40 |
| Flexural Modulus | 0.0120 - 2.69 GPa | 1.74 - 390 ksi | Average value: 0.233 GPa Grade Count:56 |
| Resilience | 0.560 - 0.750 | 0.560 - 0.750 | Average value: 0.644 Grade Count:5 |
| Flex Crack Resistance | 2.00 - 14.0 | 2.00 - 14.0 | Average value: 4.65 Grade Count:5 |
| Izod Impact, Notched | 0.530 J/cm - NB | 0.993 ft-lb/in - NB | Average value: 1.32 J/cm Grade Count:13 |
| 0.500 J/cm - NB <br>@Temperature -40.0 - -40.0 °C |
0.937 ft-lb/in - NB <br>@Temperature -40.0 - -40.0 °F |
Average value: 0.750 J/cm Grade Count:8 | |
| Izod Impact, Unnotched | NB | NB | Grade Count:7 |
| NB - NB <br>@Temperature -40.0 - -40.0 °C |
NB - NB <br>@Temperature -40.0 - -40.0 °F |
Grade Count:7 | |
| Charpy Impact Unnotched | 1000 J/cm² - NB | 4760 ft-lb/in² - NB | Grade Count:56 |
| 999.9 J/cm² - NB <br>@Temperature -30.0 - -30.0 °C |
4759 ft-lb/in² - NB <br>@Temperature -22.0 - -22.0 °F |
Grade Count:40 | |
| Charpy Impact, Notched | 1.50 J/cm² - NB | 7.14 ft-lb/in² - NB | Average value: 6.99 J/cm² Grade Count:56 |
| 0.550 J/cm² - NB <br>@Temperature -30.0 - -30.0 °C |
2.62 ft-lb/in² - NB <br>@Temperature -22.0 - -22.0 °F |
Average value: 1.35 J/cm² Grade Count:48 | |
| Tensile Creep Modulus, 1000 hours | 60.0 - 200 MPa | 8700 - 29000 psi | Average value: 113 MPa Grade Count:4 |
| Tear Strength | 38.0 - 168 kN/m | 217 - 959 pli | Average value: 91.5 kN/m Grade Count:6 |
| Taber Abrasion, mg/1000 Cycles | 46.0 - 94.0 | 46.0 - 94.0 | Average value: 71.2 Grade Count:5 |
| Compression Set | 5.00 - 62.0 % | 5.00 - 62.0 % | Average value: 30.4 % Grade Count:5 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 100 - 240 µm/m-°C | 55.6 - 133 µin/in-°F | Average value: 182 µm/m-°C Grade Count:26 |
| CTE, linear, Transverse to Flow | 100 - 210 µm/m-°C | 55.6 - 117 µin/in-°F | Average value: 169 µm/m-°C Grade Count:7 |
| Melting Point | 134 - 204 °C | 272 - 399 °F | Average value: 161 °C Grade Count:80 |
| Deflection Temperature at 0.46 MPa (66 psi) | 42.0 - 106 °C | 108 - 223 °F | Average value: 72.4 °C Grade Count:25 |
| Deflection Temperature at 1.8 MPa (264 psi) | 45.0 °C | 113 °F | Average value: 45.0 °C Grade Count:6 |
| Vicat Softening Point | 58.0 - 175 °C | 136 - 347 °F | Average value: 128 °C Grade Count:60 |
| Glass Transition Temp, Tg | -65.0 - -50.0 °C | -85.0 - -58.0 °F | Average value: -58.6 °C Grade Count:7 |
| Flammability, UL94 | HB | HB | Grade Count:28 |
| Oxygen Index | 19.4 - 22.9 % | 19.4 - 22.9 % | Average value: 20.8 % Grade Count:6 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.50 - 1.51 | 1.50 - 1.51 | Average value: 1.50 Grade Count:8 |
| Transmission, Visible | 80.0 - 90.0 % | 80.0 - 90.0 % | Average value: 80.9 % Grade Count:22 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 28.0 - 97.0 % | 28.0 - 97.0 % | Average value: 67.2 % Grade Count:6 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1000 - 1.00e+17 ohm-cm | 1000 - 1.00e+17 ohm-cm | Average value: 3.58e+15 ohm-cm Grade Count:28 |
| Surface Resistance | 0.200 - 1.00e+17 ohm | 0.200 - 1.00e+17 ohm | Average value: 2.24e+15 ohm Grade Count:45 |
| Static Decay | 1.00 sec | 1.00 sec | Average value: 1.00 sec Grade Count:4 |
| Dielectric Constant | 4.00 - 9.50 | 4.00 - 9.50 | Average value: 6.31 Grade Count:7 |
| Dielectric Strength | 5.00 - 44.5 kV/mm | 127 - 1130 kV/in | Average value: 36.1 kV/mm Grade Count:18 |
| Dissipation Factor | 0.000370 - 0.150 | 0.000370 - 0.150 | Average value: 0.0465 Grade Count:17 |
| Comparative Tracking Index | 600 V | 600 V | Average value: 600 V Grade Count:15 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 190 - 290 °C | 374 - 554 °F | Average value: 223 °C Grade Count:25 |
| Nozzle Temperature | 180 - 290 °C | 356 - 554 °F | Average value: 238 °C Grade Count:34 |
| Melt Temperature | 180 - 271 °C | 356 - 520 °F | Average value: 231 °C Grade Count:4 |
| Mold Temperature | 10.0 - 82.2 °C | 50.0 - 180 °F | Average value: 32.8 °C Grade Count:34 |
| Drying Temperature | 55.0 - 80.0 °C | 131 - 176 °F | Average value: 67.9 °C Grade Count:38 |