Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 125 °C | 257 °F | Internal method |
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h.. |
|||
Melting Point | 125 - 130 °C | 257 - 266 °F | |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300 PE 300: Polyethylene with high density. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produced by cracking of petroleum. Monom.. |
|||
Melting Point | 125 °C | 257 °F | Compression Molded; ASTM E794 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Melting Point | 125 °C | 257 °F | |
Mitsui Fybrel® UL 415 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418 |
ExxonMobil LL 8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Melting Point | 125 °C | 257 °F | ASTM E 794 |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
Melting Point | 125 - 144 °C | 257 - 291 °F | TMA Melt Range |
Huntsman IROGRAN® PS 455-204 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1150 Bicomponent HDPE/PET Fiber Type - 3 Denier X 1.5 Inches 50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni.. |
|||
Melting Point | 125 - 135 °C | 257 - 275 °F | MQSA 111 |
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low .. |
|||
Melting Point | 125 °C | 257 °F | DSC |
Lushan DE-1 Polyethylene Sintered Powder PE sintered powder Lushan DE-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PE sintered powder Lushan DE-1 is used on anti-corrosion .. |
|||
Melting Point | 125 °C | 257 °F | ASTM D2117 |
Lushan EP253H Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Melting Point | 125 - 180 °C | 257 - 356 °F | Huntsman/TMA |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium .. |
|||
Melting Point | 125 °C | 257 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M40 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-su.. |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | crystalline; DSC |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | crystalline; DSC |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | crystalline; DSC |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Melting Point | 125 - 130 °C | 257 - 266 °F | DSC |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418 |
ExxonMobil LL 8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th.. |
|||
Melting Point | 125 °C | 257 °F | ASTM-D3418 |
Braskem RA34U3 LLDPE Rotomolding Polyethylene The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418 |
ExxonMobil LL 8360 Rotational Molding Resin
(discontinued **) LL 8360 is a linear low density hexene copolymer designed to provide good processability along with outstanding dimensional control and low warpage. This resin is ideally suited for applications tha.. |
|||
Melting Point | 125 °C | 257 °F | DSC; ASTM D3418 |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |