ExxonMobil LL 8455.24 Rotational Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 8455.24 Rotational Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent dimensional control and low warpage.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
ESCR 100% Igepal® 36 hour
36 hour
ASTM D1693
ESCR 10% Igepal® 24 hour
24 hour
ASTM D1693
Melt Flow 5.5 g/10 min
5.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.03 MPa
2325 psi
ASTM D638
Elongation at Yield 17.1 %
17.1 %
ASTM D638
Flexural Modulus 0.703 GPa
102 ksi
1% secant; ASTM D790
Impact Test 70.5 J

@Thickness 3.17 mm,
Temperature -40.0 °C
52.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
156 J

@Thickness 6.35 mm,
Temperature -40.0 °C
115 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
ASTM D3418
Crystallization Temperature 109.4 °C
228.9 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C
138 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 38.0 °C
100 °F
ASTM D648
Descriptive Properties Value Comments
Features medium term UV 4 stabilization
Form PELLET