Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EM2212 PC Automotive interiors. 10% glass-reinforced. Increased stiffness/structural ridigity. High modulus/ductile. Foamed skin instrument panel uses also. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA4/6 GF30 FR HS X 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant and Heat StabilizedUL File Number: E.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 0206 Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
20.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP BF006 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BF006 is a compound based on Styrene Acrylonitrile resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 TL5 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
20.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp YF005 LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 GF13 FR 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant, Halogen Free and Impact ModifiedAppearance: BlackI.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PES GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber
(discontinued **) PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability |
|||
CTE, linear, Parallel to Flow | 36.0 µm/m-°C | 20.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 GF15 FR HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |