Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-G3U (Dry) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1 |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 25 H2.0 LT 904040 Nylon 6, 25% Glass Fiber PA 6, injection molding grade, 25% glass fibers, good heat-ageing resistance, laser-weldable |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, flame retardant |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 30.1 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30 Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-2H PA12-GF20 Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® GC30S 403 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
CTE, linear, Parallel to Flow | 30.0 - 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
16.7 - 19.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
16.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |