Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -20.0 - 150 °C |
11.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -20.0 - 150 °C |
11.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PPS 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber, 30/10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 CF40 HS 40% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 CF20 RM BK 20% Carbon Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAppearance: BlackFeatures: Low Moisture AbsorptionTPCI# 9720102Information provided by.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 L UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 G/CF20 IM HS BK 20% GlassCarbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: GlassCarbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedApp.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB36 IM1 36% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 36% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF25 HS L 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedProcessin.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF27 SL2 27% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 27% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedInformati.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HR L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated and Hydrolysis Resistant TPCI# 9357101Informatio.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HS L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 SL5 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Silicone Lubricant and Heat StabilizerFeatures: Lubricated and Heat Stabilized.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF43 L BK001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 7176101Information provi.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PEI GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS GF/M65 BK 65% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 65% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS/F GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric.. |