Polymer Property : CTE, linear, Parallel to Flow = 28.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
CTE, linear, Parallel to Flow 28.0 µm/m-°C
15.6 µin/in-°F
ASTM D696
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose
Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East)
Internally lubricated PA6.12, containing Glass Fiber and PTFE
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY
Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3..
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, DRY
Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors ..
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 28.0 µm/m-°C
15.6 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66  (Unverified Data**)
30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 28.0 µm/m-°C
15.6 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66  (Unverified Data**)
Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded
AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 20.0 °C
15.6 µin/in-°F

@Temperature 68.0 °F
Covestro Bayblend® KU 2-1466 Polycarbonate/ABS Blend
Flame retardant grade with 20% glass fiber reinforcement, high stiffness.Applications: Electrical industry.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated f..
CTE, linear, Parallel to Flow 28.0 µm/m-°C
15.6 µin/in-°F
ISO 11359
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry)
Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the..
CTE, linear, Parallel to Flow 28.0 µm/m-°C
15.6 µin/in-°F
ISO 11359
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT
Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement.
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10
LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive.