Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ASTM D696 |
PolyOne Edgetek® PC-15CF/000 FCR Polycarbonate (PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler
(discontinued **) Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon OCL13 PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13 is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 °C |
7.78 µin/in-°F @Temperature 73.4 °F |
TMA |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
7.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DC0041PQ PC LNP* THERMOCOMP* DC0041PQ is a compound based on Polycarbonate resin containing Carbon Fiber. Added feature of this grade is: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | TMA |
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic Novolac resin based, glass fiber and mineral filled. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in particular in the ABS system.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | TMA |
Vyncolit X659 Glass, Mineral and Graphite Filled Novolac Phenolic Novolac resin based, glass fiber, mineral and graphite filled. Grade with superior stiffness, high dimensional stability and excellent tribological properties. Good chemical resistance against sever.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | TMA |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | TMA |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-60 FC PA6-GF60 Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 55.0 - 160 °C |
7.78 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)
(Unverified Data**) 55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ACF6 PA66, 30% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF6 is a 30% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
7.78 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2650 Z6 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grade for applications requiring the highest impact strength together with low stiffness.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 14.0 - 16.0 µm/m-°C @Temperature 50.0 - 150 °C |
7.78 - 8.89 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 20.0 °C |
7.78 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C | 7.78 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |