Material Notes:
This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tapes become highly crystalline and lose their desirable elastomeric properties. Interleave: 3 mil PE; Rubber: Cured self fusing silicone.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Arlon SQA-TMS-024
Water Absorption 0.40 %
0.40 %
MIL-I-46852C
Thickness 508 microns
20.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ASTM D2240
Tensile Strength, Ultimate 6.55 MPa
950 psi
ASTM D412
Elongation at Break 425 %
425 %
ASTM D412
Adhesive Bond Strength 0.0152 MPa
2.20 psi
MIL-I-46852C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -116 °C
-177 °F
Arlon SQA-TMS-055
Electrical Properties Metric English Comments
Dielectric Strength 27.6 kV/mm
700 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments