Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 757 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 757SSG (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VH (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VHF (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 774VHF-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-1S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-2S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-3S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-4S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants PG-8S Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants UniFlor 8322 (857A) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | impact conditions and heavy loads not considered |
Omnia Plastica PP Polypropylene The mechanical features of PP are better than those of PE H.D. It withstands attack by alkali and acids and consequently it is widely used for components in the chemical industry when a moderate str.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | T10 |
Precision Polymer Engineering N60R Nitrile Rubber Red Nitrile Butadiene / PVC elastomer blend 59-65°IRHD. Electrically non-conductive. Copolymer of acrylonitrile and butadiene, blended with polyvinyl chloride.Applications: Specially formulated as .. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V60F Fluoroelastomer Compound Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line c.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V70A Fluoroelastomer Compound Blue Fluoroelastomer Rubber, 65-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2, where Z1 = comp-.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V75F Fluoroelastomer Compound Special steam resistant, Fluoroelastomer Rubber, 70-80 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V80H Fluoroelastomer Compound Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Federal Food and Drug Adminis.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V97B Fluoroelastomer Compound Fluoroelastomer Rubber, 90-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out M3HK914, A1-10, B37, B38, EF31, EO78, Z1. Wher.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
Precision Polymer Engineering V97D Fluoroelastomer Compound Fluoroelastomer Rubber, 92-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. Tested at the Shell Thornton Research Centre, where it has shown excellent res.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
Nye Lubricants 875R (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Continuous; DIN 52612 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | |
ChevronTexaco Dura-Lith® NLGI 3 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | TR test, TR70 |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | TR test, TR70 |
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | ASTM D 3575 |
Eurofoam Evacell EVA 100 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | ASTM D 3575 |
Eurofoam Evacell EVA 200 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Service |
3M 3000WT Fire Barrier Water Tight Sealant 3M Fire Barrier Water Tight Sealant 3000 WT is a high-performance, ready-to-use, single component, neutral cure, non-slumping intumescent silicone sealant. Product cures upon exposure to atmospheric.. |
|||
Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Application |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |