Material Notes:
Fluoroelastomer Rubber, 92-98 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. Tested at the Shell Thornton Research Centre, where it has shown excellent resistance to explosive decompression (ED) under a known range of conditions. ASTM designation = FKM. ISO designation = FPM.Applications: Approved and specified by Shell for use in applications where ED conditions exist. ED occurs when low molecular weight gas atmospheres are reduced from high to low pressure in a short period of time.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
°IRHD; ASTM D1415
Tensile Strength, Yield 11.8 MPa
1710 psi
ASTM D412
Elongation at Break 100 %
100 %
ASTM D412
Compression Set 40 %
40 %
168 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Flash Point >= 315 °C
>= 599 °F