Material Notes:
3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair holes and tears in these building materials. Taping seams aids in reducing air infiltration, improving the effectiveness of insulation and reducing heating and cooling costs.Information provided by 3M
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Backing; ASTM D3652
76.2 microns
3.00 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.1 MPa
6690 psi
ASTM D3759
Elongation at Break 130 %
130 %
ASTM D3759
Peel Strength 0.175 kN/m
1.00 pli
Adhesion to Polyethylene; ASTM D3330
0.27391 kN/m
1.5625 pli
Adhesion to Housewrap; ASTM D3330
0.49303 kN/m
2.8125 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
105 °C
221 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
-10.0 °C
14.0 °F
Application
Descriptive Properties Value Comments
Adhesive Type Acrylic
Appearance Red