Precision Polymer Engineering V60F Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V60F Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Peroxide/Litharge cured, Fluoroelastomer Rubber, 55-65 °IRHD. Tetrapolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene and cure site monomer (CSM). To meet ASTM D2000 line call-out: MHK610, A1-10, B37, B38, EF31, EO78. ASTM designation = FKM. ISO designation = FPM.Applications: Alcohol blended fuel systems (methanol or gasohol), SF/SG engine oils, phosphate ester fluids, acids, hot water and steam. Chemical resistance superior to other FKM’s.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
70
70
°IRHD, +10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
-25% change after 72 hours @ 250°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 150 %
150 %
-25% change after 72 hours @ 250°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 30 %
30 %
22 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Flash Point >= 315 °C
>= 599 °F