| Category | Fluid , Lubricant , Aluminum Gellant , Organic Soap Gellant , Polyalphaolefin (PAO) |
| Manufacturer | Nye Lubricants |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Nye Lubricants PG-4S Grease.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 53 cSt | 53 cSt | Base Oil; ASTM D445 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 85 | 85 | ASTM D217 |
| Oil Separation | 0.50 % | 0.50 % | 24 hrs, 100C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 125 °C | 257 °F | Recommended |
| Minimum Service Temperature, Air | -10.0 °C | 14.0 °F | Recommended |
| Pour Point | -20.0 °C | -4.00 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | PAO | |
| Gellant Type | Al. Stearate |