Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants 380C (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants 774VLF-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants UniFlor 8130 (475) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants UniFlor 8132 (832) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
Nye Lubricants UniFlor 8511R (853RP-2) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Precision Polymer Engineering R70D Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 70 (NRQX70).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Cured |
Resin Technology Group CT-523LV Cationic UV Cure Epoxy Adhesive CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical re.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Termopol Termoton® V5GA1090A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
GEHR Plastics PPSU Polyphenylenesulfone Polyphenylenesulfone is an amorphous material, with improved impact and hydrolysis resistance compared to PSU. The usual operating temperature is approximately 180°C. The extremely high notched i.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Zeus THV Tubing THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Dow Corning 752 ADHESIVE/SEALANT General purpose silicone adhesive/sealantInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Dow Corning MOLYKOTE® PG-54 PLASTISLIP GREASE Silicone grease with solid lubricantsInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 400901S SBS Based Material, 90A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 660850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Dryflex® 662850S SEBS Based Material, Semi-Filled Qualities, 85A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Mediprene™ 500750M TPE, Medical Applications, 75A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
Adamas Adalon® 509 PTFE, 3% MoS2 Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
Adamas Adalon® 413 PTFE, 20% PPS Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
Atom Adhesives AA-DUCT 906 Epoxy Adhesive AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
3M 8429 Polyester Tape 3M™ Polyester Tape 8429 is composed of a heavy duty polyester backing with an aggressive, versatile rubber adhesive. The polyester backing in strong yet thing making it ideal for demanding applicat.. |
|||
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous; DIN 52612 |
Isoflon PA 11 Polyamide 11 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |