ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mechanical properties, such as elongation, compression set, tensile and tear strength. The low density entails lower weight compared to the 600 and 660-series.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 65

@Thickness 4.00 mm
65

@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
100% Modulus 0.00200 GPa
0.290 ksi
ASTM D638
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
Tear Strength 28.0 kN/m
160 pli
ASTM D624
Compression Set 20 %
20 %
at 23°C, 72 hrs; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F
Descriptive Properties Value Comments
Bonding to PP Excellent
Chemical Resistance Good
Excluding organic solvents, aromatic and vegetable oils
Color Translucent
Weather Resistance Excellent
Air ageing