Dow Corning 752 ADHESIVE/SEALANT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 752 ADHESIVE/SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose silicone adhesive/sealantInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc

@Temperature 25.0 °C
1.03 g/cc

@Temperature 77.0 °F
Volatiles 3.0 %
3.0 %
Mechanical Properties Metric English Comments
Hardness, Shore A 24
24
Tensile Strength, Ultimate 2.40 MPa
348 psi
Die 3
Elongation at Break 490 %
490 %
Tear Strength 4.38 kN/m
25.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Shelf Life 27.0 Month
27.0 Month
Descriptive Properties Value Comments
Appearance clear
Color Black
White