Material Notes:
CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low outgassing polymer system capable of surviving exposure up to 200°C.Applications: Disk drive engineering products, non-acrylic UV bonding. No out gassing concerns. Use as conformal coat and/or wire tack. Opto-Electronic, Fillet-tacking and staking.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Viscosity 3300 cP

@Temperature 25.0 °C
3300 cP

@Temperature 77.0 °F
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Cured
Tensile Strength at Break >= 34.5 MPa
>= 5000 psi
Cured
Shear Strength 15.2 MPa
2200 psi
Cured, lap
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Cured
Descriptive Properties Value Comments
Color Clear
Composition Epoxy
Moisture Resistance Excellent
Cured
Toxicity Low