Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 90
90
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 23 cSt
23 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.0 cSt
4.0 cSt
Base Oil; ASTM D445
Evaporation Loss 2.5 %
2.5 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 316
316
ASTM D217
Penetration P(60), 1/10 mm 339
339
ASTM D217
Oil Separation 8.7 %
8.7 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Recommended
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Recommended
Pour Point -63.0 °C
-81.4 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(pnd)
Gellant Type PTFE
Users viewing this material also viewed the following: