Polymer Property : Vicat Softening Point = 347 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 175 °C

@Load 5.001 kg
347 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYshine PBT D223 Q30 FR PBT, Mineral Reinforced, Flame Retardant
Information provided by Polykemi AB
Vicat Softening Point 175 °C
347 °F
ASTM 1525-00 modified
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant
Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
Vicat Softening Point 175 °C
347 °F
ASTM 1525-00 modified
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
Vicat Softening Point 175 °C
347 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific)
LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci..
Vicat Softening Point 175 °C
347 °F
ASTM 1525-00 modified
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant
Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica..
Vicat Softening Point 175 °C
347 °F
ASTM 1525-00 modified
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
Vicat Softening Point 175 °C

@Load 5.00 kg
347 °F

@Load 11.0 lb
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East)
Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem HATX100 PEI+PCE
Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific)
Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Vicat Softening Point 175 °C
347 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Vicat Softening Point 175 °C
347 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Vicat Softening Point 175 °C
347 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Vicat Softening Point 175 °C
347 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® V4860HR PBT
30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® VX5121 PBT (Europe-Africa-Middle East)
VALOX VX5121 is a 15 % glass reinforced PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Vicat Softening Point 175 °C
347 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Vicat Softening Point 175 °C
347 °F
50°C/h 50N; ISO 306
DuPont Performance Polymers Crastin® CE2055 NC010 Polybutylene Terephthalate (PBT)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin CE2055 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Perf..
Vicat Softening Point 175 °C

@Load 1.02 kg
347 °F

@Load 2.25 lb
ISO 306
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Vicat Softening Point 175 °C

@Load 1.02 kg
347 °F

@Load 2.25 lb
ISO 306
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..