Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 158 °C | 316 °F | B |
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 158 °C | 316 °F | ASTM D1525 |
PolyMirae Moplen HP640G Sheet and Thermoforming Grade Polypropylene Moplen HP640G is the polypropylene Homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640G is a homopolymer particularly suitable for sheet and thermof.. |
|||
Vicat Softening Point | 158 °C | 316 °F | 50°C/h 50N; ISO 306 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Vicat Softening Point | 158 °C | 316 °F | 50°C/h 50N |
Covestro Apec® DP 1-9339/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Vicat Softening Point | 158 °C | 316 °F | |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Vicat Softening Point | 158 °C | 316 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 160D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 158 °C | 316 °F | |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Vicat Softening Point | 158 °C | 316 °F | ASTM D1525 |
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306/B50 |
Styron CALIBREâ„¢ 5201-12 Polycarbonate Resin Overview: CALIBREâ„¢ 5201-12 polycarbonate resin is 20% glass reinforced containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. CALI.. |
|||
Vicat Softening Point | 158 °C | 316 °F | A (10 N); ISO 306 |
Borealis Bormod™ HD905CF Polypropylene Homopolymer for Cast Film Bormod HD905CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, suitable for the manufacturing of unoriented film on chill roll process. It is recomme.. |
|||
Vicat Softening Point | 158 °C | 316 °F | A (10 N); ISO 306 |
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s.. |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® NB 108 Polypropylene Homopolymer Applications include injection molding and fibers. Basic and anti-gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® TL 003 Polypropylene Homopolymer Made for tape applications. UV stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® GH 005 Polypropylene Homopolymer Made for injection molding. LTHA stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® MT 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | 50°C/h 50N |
Covestro Texin® 270 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Vicat Softening Point | 158 °C | 316 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Vicat Softening Point | 158 °C | 316 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber This material has good hot water resistance and sliding properties. Its applications include seals, scrapers and chain guides, and toothed wheels and rollers.Information provided by CENTROPLAST Eng.. |
|||
Vicat Softening Point | 158 °C | 316 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1040 PP SABIC® PPcompound 15T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound, suitable for injection molding applications. The IMDS ID is 16487994 |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Vicat Softening Point | 158 °C | 316 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | ISO 306 |
Unipetrol PP MONSTEN® GB 003 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 158 °C | 316 °F | -1kg; ASTM D1525 |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |