Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 150 °C | 302 °F | ASTM D1525B |
SABIC PP 413MNK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 413MNK45 is a controlled rheology PP grade with a very high fluidity. It is provided with an antistatic package & nucleating agent and is especially developed for producing.. |
|||
Vicat Softening Point | 150 °C | 302 °F | ASTM D1525B |
SABIC PP 528K Polypropylene Homopolymer for Thermoforming Product Description: PP 528K is formulated with an advanced nucleating additive and was specially developed for in-line and off-line thermoforming applications. PP528K exhibits the following featu.. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 955 PC (Europe-Africa-Middle East) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Vicat Softening Point | 150 °C @Load 5.10 kg |
302 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® S USX200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® PK2870 PC LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Vicat Softening Point | 150 °C | 302 °F | ASTM D1525 |
Hyosung Topilene B200 PP B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation |
|||
Vicat Softening Point | 150 °C | 302 °F | ASTM D1525 |
Hyosung Topilene HJ145 PP HJ145 High Isostatic PP Impact CopolymerApplications:Low pressure injection moldingAutomobile partsCharacteristics:High flowabilityHigh stiffnessMedium impactInformation provided by Hyosung Corporat.. |
|||
Vicat Softening Point | 150 °C | 302 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® 24 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 150 °C | 302 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 150 °C @Load 5.10 kg |
302 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Vicat Softening Point | 150 °C @Load 5.00 kg |
302 °F @Load 11.0 lb |
|
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Vicat Softening Point | 150 °C @Load 5.00 kg |
302 °F @Load 11.0 lb |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Vicat Softening Point | 150 °C | 302 °F | 10N, 50°C/hr; ISO 306 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Vicat Softening Point | 150 °C | 302 °F | 50°C/hr, 50N; ISO 306-B50 |
Styron CALIBREâ„¢ 7100-8 Polycarbonate CALIBREâ„¢ 7100-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Vicat Softening Point | 150 °C | 302 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Vicat Softening Point | 150 °C @Load 1.02 kg |
302 °F @Load 2.25 lb |
50% humidity, 23°C; ISO 306 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Vicat Softening Point | 150 - 155 °C | 302 - 311 °F | Softening point range is 150-155°C. Method not specified. |
Total PPH 3762 Polypropylene, Extrusion Grade Homopolymer fiber grade for staple fiber and multifilament yarnsFading Resistance - FINA 3762 is formulated to resist gas fading while maintaining excellent processing stability up to 250oC.Process .. |
|||
Vicat Softening Point | 150 °C | 302 °F | A50 (10N); ISO 306 |
Domo 2300K Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 150 °C @Load 1.02 kg |
302 °F @Load 2.25 lb |
ASTM D1525 |
Carmel Olefins CAPILENE® SL 50 Polypropylene Impact Copolymer Description: CAPILENE® SL 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade combines good stiffness and impact properties.Applications: CAPILENE® SL .. |
|||
Vicat Softening Point | 150 °C | 302 °F | ISO 306 |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Vicat Softening Point | 150 °C | 302 °F | ISO 306 |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Vicat Softening Point | 150 °C | 302 °F | ISO 306 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Vicat Softening Point | 150 °C | 302 °F | VST/B/50; ISO 306 |
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin.. |
|||
Vicat Softening Point | 150 °C @Load 1.00 kg, Thickness 4.00 mm |
302 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Vicat Softening Point | 150 °C | 302 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |
|||
Vicat Softening Point | 150 °C | 302 °F | ASTM D1525 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |