Eastman D4041-P Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman D4041-P Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low-density polyethylene D4041-P is a recommended for use in the boardstock coating industry for applications such as breadboard, cupstock, and liquid packaging board. This resin has low neck-in and good drawdown characteristics. Coatings produced from it exhibit excellent heat-sealing characteristics.List of Applications:Food-contact applicationsPhotographic paperInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D4883
Melt Flow 5.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 MPa
1310 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 13.1 MPa
1900 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 180 %
180 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.255 GPa
37.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating