Material Notes:
ApplicationsPETROTHENE NA831-000 resin exhibits high stress crack resistance and low temperature brittleness. Typical applications include housewares, containers and industrial parts. Regulatory StatusNA 831-000 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520C 2.1. This regulation allows the use of this olefin polymer in "…articles that contact food except for articles used for packing or holding food during cooking." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 831-000 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus 0.255 GPa
37.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C
104 °F
ASTM D648
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Brittleness Temperature -65.0 °C
-85.0 °F
F<sub>50</sub>; ASTM D746