Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.50 GPa | 798 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 49 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | |
Plastcom SLOVAMID 66 GF 15 T 25 PA66, 15% glass fibre, 25% talc FeaturesChemically reinforced with 15% glass fibre and talc, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical in.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 5.50 GPa @Temperature 23.0 °C |
798 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D223 GF10 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.50 - 6.50 GPa | 798 - 943 ksi | ISO 178 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene
(discontinued **) ABS glass fiber filled, excellent mechanical properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
Loxim 315 01HB Nylon 6 Information provided by Loxim Industries |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/GY Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2mm/min; ASTM D790 |
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF004 Acetal Copolymer (Europe-Africa-Middle East) LNP* THERMOCOMP* KF004 is a compound based on Acetal Copolymer containing Glass Fiber. Added features include : Chemically Coupled. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
Polyram RamTough PZ307G4 Polycarbonate, 20% Glass Fiber, UV Stabilized 20% glass fiber reinforced polycarbonate, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
Polyram PlusTek PB825G5 Nylon 6, 25% Glass Fiber 25% glass fiber reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.50 GPa @Temperature 160 °C |
798 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF003S PA66, 15% Glass Fiber Filled, Injection Molded Staramide RF003S is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PX06010 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06010 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP KUR 1060 GFC Polypropylene, 30% Glass Filled PP copolymer 30% chemically coupled glass fiberElastomer modified, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
Eurotec® Tecodur® PB70 GR15 NL PBT 15% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 3412ECR PC Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO Data |
BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET Ultradur B 4040 G3 HT BK5830 is a 15% glass filled, pigmented black, injection molding PBT. It is a resin for molding household appliances and equipment which must be resistant to chemicals and oth.. |
|||
Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
CENTROPLAST CENTROLEN PP GF 30 Polypropylene 30% glass fiber This material is a low density, easily machined plastic that has high impact resistance and dimensional stability. Applications include air filter housings, fan blades, and fittings with high loads... |