Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | STN EN ISO 178 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D234 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific) Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT C213 GF15 FR PBT, Glass Fiber-Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, Conditioned Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Unitika M1030E PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Polyram RamShine PW311G4 SAN, 20% Glass Fiber 20% Glass fiber reinforced SAN for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | dry; ISO 178 |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Adell BH-18 Nylon 6, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO Data |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® ABS Resin R2018, 18% Glass Reinforced General purpose, 18% glass reinforced ABS resin.Data provided by the manufacturer |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520-20GU Nylon 66, 20% Glass Reinforced 20% Glass reinforced Nylon 66, utility grade.Data provided by the manufacturer |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO Data |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |