Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.50 GPa | 653 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 66 GF 20 PA66 reinforced with glass fiber PA66 reinforced with 20 % glass fiber, used in the automotive, engineering and electrical industry. Application: hobby tools, covers of electrotools, electromotors, cooling screws of blowers, gear w.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
Niche Polymer PA66MI40N Nylon 66, 40% Mineral Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B32^ E F15 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178/1A |
Radici Raditer® B RV 150 Polybutylene Terephthalate with 15% Glass fiber Raditer® B RV 150 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
Gichem GILAC A50VX35/VO ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0, 17% glass fiber filled, good stiffness. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | |
Lehmann & Voss LUVOCOM® 1-8520 Polyamide 66, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | |
Kuraray Genestarâ„¢ TA104 Nylon Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM-D790 |
Polyram Polytron P20B01 Homopolymer Polypropylene, Chemically Coupled 20% Long Fiber A CHEMICALLY COUPLED 20% LONG FIBER GLASS REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | DAM; ISO 178 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |
|||
Flexural Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM-D790 |
Polyram RamSter PF353M6 PBT, 30% Mineral Filled 30% mineral filled for injection molding applicationsInformation provided by Polyram Ram On Ind. |