Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | |
Plastcom SLOVALEN PH 51 T 30 PP, 30% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.5mm/min; ISO 178:2001 |
Nylacast Aquanyl Nylon 612 Copolymer Aquanyl is a copolymer of Nylon 6 and Nylon 12 produced via the anionic polymerization process using the monomer's Caprolactam and Laurinlactam. It has reduced water absorption, improved stability a.. |
|||
Flexural Modulus | 2.70 - 3.30 GPa | 392 - 479 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
Nilit FRIANYL B63 UF Nylon 6 for injection molding Nylon 6 for injection molding, highly crystallized, UV stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYform POM C M140 Polyoxymethylene Information provided by Polykemi AB |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX7189 PC Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Faradex DS0036IC PC (Europe-Africa-Middle East) LNP* FARADEX* DS0036IC is a compound based on Polycarbonate resin, containing Stainless Steel Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, High I.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
Styrolution Novodur® HH-112 ABS Novodur HH-112 is a high heat injection molding grade. It provides good heat resistance combined with enhanced stiffness.Information provided by Styrolution |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178 |
Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide Nylon 66 with molybdenum disulfide, low friction and high abrasion resistance, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178-93 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ISO 178-93 |
Wellman Wellpet® PR109-N1 Unfilled PET Description: Unfilled PETInformation provided by Wellman. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | dry; ISO 178 |
DSM Akulon® K123, K123/A PA6 Low Viscosity |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Loxim 400 00HB Nylon 6,6 Information provided by Loxim Industries |
|||
Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |