Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® K123, K123/A PA6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® K123, K123/A PA6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low Viscosity
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
dry; ISO 1183
Water Absorption 9.5 %
9.5 %
Sim. To ISO 62
Moisture Absorption 2.50 %
2.50 %
Sim. To ISO 62
Viscosity Test 135 cm³/g
135 cm³/g
Viscosity Number; ISO 307, 1157, 1628
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.2 MPa
10900 psi
dry; ISO 527-1/-2
Elongation at Break 30 %
30 %
dry; ISO 527-1/-2
Tensile Modulus 2.80 GPa
406 ksi
dry; ISO 527-1/-2
Flexural Modulus 2.70 GPa
392 ksi
dry; ISO 178
Izod Impact Resistance 0.699 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 180/1A
Charpy Impact, Notched 0.699 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
dry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
dry; ISO 75-1/-2