Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.39 GPa | 347 ksi | ASTM D790 |
Omni Plastics OmniTech™ PA6/6,6 V2 125 IM8 Flame Retardant OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXG154 PC FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXM941A PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | ASTM Data |
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and che.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | ASTM D790 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 195 PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 195HP PBT PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 3-point, 2 mm/min; ISO 178 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Europe-Africa-Middle East) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3003MC Black 1722 Description: BlackInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | ASTM D790 |
BASF Ultramid® BG50XFI PA6 (Dry) Description: Ultramid BG50XFI is an impact modified, injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | ASTM Data |
BASF Capron® BG50XFI Impact Modified Nylon 6 (Dry)
(discontinued **) Capron BG50XFI is an injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths. It is also available in natura.. |
|||
Flexural Modulus | 2.39 GPa | 347 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |