Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific) AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 945AU PC Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 945AU PC (Asia Pacific) Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 955AU PC (Asia Pacific) Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EX1632T PC Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available .. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXD121R PC (Asia Pacific) Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXG121R PC PC in special effects colors. ""Diamond Sparkle"" appearance additives. Color package may affect performance. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX1832 PC MFR=3.0; Branched extrusion grade for LED applications, UV stabilized; available in diffuse colors |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML6076 PC Passes FAR 25.853: 60 seconds at 30 mil. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® OQ3732 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized PC for ophthalmic lenses. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925A PC Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925A PC (Asia Pacific) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925AU PC Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 945A PC Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® ML4248 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Extrusion grade. Transparent, transluscent and opaque colors. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly LNP* LUBRICOMP* KL002 is a compound based on Acetal Copolymer resin containing 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | Injection Molded; ASTM D790 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Flexural Modulus | 2.37 GPa | 344 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 2.37 GPa @Thickness 3.17 mm |
344 ksi @Thickness 0.125 in |
chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 4107 Heat Resistant Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |