| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 | 
| Melt Flow |           2.2           g/10 min           @Load 3.80 kg, Temperature 230 °C  | 
                  2.2           g/10 min           @Load 8.38 lb, Temperature 446 °F  | 
        ASTM D1238 | 
|           3.6           g/10 min           @Load 10.0 kg, Temperature 220 °C  | 
                  3.6           g/10 min           @Load 22.0 lb, Temperature 428 °F  | 
        ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 44.1 MPa | 6400 psi | chs 2 in/min; ASTM D638 | 
| Elongation at Break | 11 % | 11 % | chs 2 in/min; ASTM D638 | 
| Flexural Strength |           68.8           MPa           @Thickness 3.17 mm  | 
                  9980           psi           @Thickness 0.125 in  | 
        chs 0.05 in/min; ASTM D790 | 
| Flexural Modulus |           2.37           GPa           @Thickness 3.17 mm  | 
                  344           ksi           @Thickness 0.125 in  | 
        chs 0.05 in/min; ASTM D790 | 
| Izod Impact, Notched |           0.961           J/cm           @Thickness 6.35 mm  | 
                  1.80           ft-lb/in           @Thickness 0.250 in  | 
        ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Vicat Softening Point |           134           °C           @Load 1.00 kg, Thickness 3.17 mm  | 
                  273           °F           @Load 2.20 lb, Thickness 0.125 in  | 
        ASTM D1525 |