SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copoly (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 9.7 %
9.7 %
ASTM D638
Tensile Modulus 2.55 GPa
370 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.37 GPa
344 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.64 J/cm
10.6 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C

@Thickness 3.20 mm
198 °F

@Thickness 0.126 in
unannealed; ASTM D648