Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.76 GPa | 255 ksi | Tangent; ASTM D790 |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Omni Plastics OmniTuff™ CPP CCF30 Copolymer Polypropylene Calcium Carbonate Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Polymer Resources PPX-GP4 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6 Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH120LN Polypropylene, Homopolymer, Injection Molding, Antistat/Lube COPYLENE™ CH120LN is designed for general purpose injection molding applications with anti-static and nucleation. Applications: Food Containers, Housewares, Closures.Information provided by Phillip.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH350LN Polypropylene, Homopolymer, High Flow, Nucleated, Lube, Injection Molding COPYLENE™ CH350LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio.. |
|||
Flexural Modulus | 1.76 - 2.80 GPa | 255 - 406 ksi | Average value: 2.26 GPa Grade Count:56 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 1.76 - 3.40 GPa | 255 - 493 ksi | Average value: 2.41 GPa Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH200LN Polypropylene, Homopolymer, CR, Antistat, Nucleated, Injection Molding COPYLENE™ CH200LN is designed for general purpose injection molding applications with anti-static, nucleation and controlled rheology. Applications: Food Containers, Housewares, Closures.Informatio.. |
|||
Flexural Modulus | 1.76 - 22.5 GPa | 255 - 3260 ksi | Average value: 16.4 GPa Grade Count:9 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
M. Holland Company PP710 Polypropylene Homopolymer AntistaticHomopolymerNarrow molecular wt. dist.NucleatedApplications: CapsClosuresConsumer applications |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D790 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D 790 |
Styrolution PS 5310 HIPS Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D 790 |
Styrolution PS 7120 HIPS Excellent ESCR to foodstuffs and PUR foamsGood low temperature impact strengthHigh relative stiffness/potential to down gauge sheetUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX6010 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | Tangent; ASTM D790 |
Washington Penn Homopolymer Polypropylene 10% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.76 GPa | 255 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem FT200WV Homopolymer Polypropylene Description: Good mold release, nucleated, excellent rigidity and hardness.Applications: Suggested uses include housewares, caps and closures, fast-cycle injection molding.Process: Injection Molding.. |