Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.0 - 17.0 GPa | 1890 - 2470 ksi | Compression; ISO 178 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Flexural Modulus | 13.0 - 16.0 GPa | 1890 - 2320 ksi | Compression; ISO 178 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Flexural Modulus | 13.0 - 16.0 GPa | 1890 - 2320 ksi | Injection; ISO 178 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Cookson Group Plaskon® S-7S Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Cookson Group Plaskon® SMT-B-1RC (146.403) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
IDI Composites 46-16-60 Thermoset Polyester, Sheet TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
IDI Composites C-204 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
IDI Composites M-106 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
IDI Composites M-207 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Lehmann & Voss LUVOCOM® 1-1119-1 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 13.0 GPa @Temperature 100 °C |
1890 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific) 9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ISO 178 |
Vyncolit 2940 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. USES: Multi-V pulleys and solenoid covers.Information provided by Vyncolit, a Sumitomo Bak .. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | |
Cytec Thornel® Graphite Cloth Laminate with Mil R-9299 Resin Data provided by the manufacturer, Amoco Performance Products, Inc.Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperature.. |
|||
Flexural Modulus | >= 13.0 GPa | >= 1890 ksi | IEC 1212-2 5.2 |
Hippe SI GC 201 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in electrical and electronic applications. Extremely good electrical properties under dry conditions; good properties under humid conditions.Information provided by Hippe. |
|||
Flexural Modulus | >= 13.0 GPa | >= 1890 ksi | IEC 1212-2 5.2 |
Hippe SI GC 202 Woven Glass Cloth Reinforced Silicone Resin - Sheet Used in mechanical and electrical applications at elevated temperature. Good heat resistance.Information provided by Hippe. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ISO 178 |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |