| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.98 g/cc | 0.0715 lb/in³ | ASTM D792 |
| Water Absorption | 0.090 % | 0.090 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
| Flexural Strength | 111 MPa | 16100 psi | ASTM D790 |
| Flexural Modulus | 13.0 GPa | 1890 ksi | ASTM D790 |
| Compressive Strength | 164 MPa | 23800 psi | ASTM D695 |
| Shear Strength | 21.0 MPa | 3050 psi | ASTM D732 |
| Izod Impact, Notched | 2.80 J/cm | 5.25 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 4.19e+14 ohm | 4.19e+14 ohm | Insulation Resistance, Condition A, ASTM D257 |
| Dielectric Constant | 4.85 @Frequency 1e+6 Hz |
4.85 @Frequency 1e+6 Hz |
Condition A, ASTM D150 |
| 6.58 @Frequency 60 Hz |
6.58 @Frequency 60 Hz |
Condition A, ASTM D150 | |
| Dielectric Strength | 11.0 kV/mm | 279 kV/in | Short-Term; ASTM D149 |
| Dissipation Factor | 0.018 @Frequency 1e+6 Hz |
0.018 @Frequency 1e+6 Hz |
Condition A, ASTM D150 |
| 0.024 @Frequency 60 Hz |
0.024 @Frequency 60 Hz |
ASTM D150 | |
| Arc Resistance | 199.5 sec | 199.5 sec | Condition A, ASTM D495 |