Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.9 GPa | 1870 ksi | ASTM D790 |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 CF30 TL12 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance and Lo.. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ISO 178-93 |
Wellman Wellamid® GFX1743-BK1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6 Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ISO 178-93 |
Wellman Wellamid® GFX1743-N1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6 Description: Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6Information provided by Wellman. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11427 LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G.. |
|||
Flexural Modulus | 12.9 GPa | 1870 ksi | ISO Data |
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry) Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness. |