Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 171 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.18 GPa
171 ksi
at 1% Secant; ASTM D790
NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin
Good balance of physical and molding properties-high toughness, Excellent processability on high-speed, multiple-head blow molding lines, UL-94HB listedApplications: Household chemical bottles, Indu..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
PolyMirae Moplen EP340G Sheet and Thermoforming Grade Polypropylene
Moplen RP340G is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340G is a random copolymer particularly suitable for..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
PolyMirae Moplen EP301C Pipe Extrusion/ Sheet/ Blown Film Grade Polypropylene
Moplen EP301C is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP301C is a block copolymer suitable for industrial pipe and se..
Flexural Modulus 1.18 GPa
171 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar..
Flexural Modulus 1.18 GPa
171 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..
Flexural Modulus 1.18 GPa
171 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..
Flexural Modulus 1.18 - 13.8 GPa
171 - 2000 ksi
Average value: 9.49 GPa Grade Count:167
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene B240 PP
B240 Extrusion Impact CopolymerApplications:Corrugated sheetThick sheetCharacteristics:High impactInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene B240P PP
B240P Extrusion Impact CopolymerApplications:Pipe (drain, etc…)Characteristics:Pressure resistanceHigh impactLong-term heat stabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene J440 PP
J440 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene J640 PP
J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene J640U PP
J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene R301 PP
R301 Extrusion Random CopolymerApplications:Extrusion blow moldingThermoforming sheetCharacteristics:TransparencyStiffnessStretchabilityInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene R401 PP
R401 Extrusion Random CopolymerApplications:Extrusion blow moldingStationary sheetCharacteristics:TransparencyStiffnessInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Hyosung Topilene R801 PP
R801 Injection Random CopolymerApplications:High transparent productLarge articlesCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation
Flexural Modulus 1.18 GPa

@Thickness 6.40 mm
171 ksi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL EI5002 PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
LG Chemical SEETEC PF150 HDPE
Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D760
LG Chemical SEETEC R1610 Polypropylene Random Copolymer
Features: SEETEC R1610 is a highly transparent ethylene-propylene random copolymer for injection molding applications. SEETEC R1610 exhibits an excellent transparency and a good impact strength. SEE..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790B
Lotte Chemical Titan TITANPRO® SM240 Polypropylene impact copolymer
Titanpro® SM240 is a high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet ..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding
Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, sof..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding
Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P750J Polypropylene Injection Molding
Key Characteristics:Excellent clarityHigh productivityGood processability and stiffnessHigh glossOdorlessSafe for food contactRecommended Applications:Food container, utensilMedical parts such as sy..
Flexural Modulus 1.18 GPa
171 ksi
0.039 in/min; ISO 178
ExxonMobil Exxtral™ BMU130A Performance Polyolefin
Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailabilit..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Equate EMDA-6147 HDPE Blow Molding Resin
EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density..
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou..
Flexural Modulus 1.18 GPa
171 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Rilsamid® PA 12 AESNO MED Nylon 12
Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the..
Flexural Modulus 1.18 GPa
171 ksi
ISO 178
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry)
Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf..
Flexural Modulus 1.18 GPa
171 ksi
ASTM-D-790
BCC Products LIK-WOOD BC 8007 Urethane Casting
Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an..
Flexural Modulus 1.18 GPa
171 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON MS000IL PP
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c..
Copyright © lookpolymers.com All Rights Reserved