Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, soft drink, milk, detergent, cosmetics products, lube oil, brake fluid, chemicalsInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.958 g/cc
0.958 g/cc
ASTM D1505
Environmental Stress Crack Resistance 300 hour

@Temperature 50.0 °C
300 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 27.0 MPa
3920 psi
ASTM D638
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Break 1000 %
1000 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 132 °C
270 °F
ASTM D2117
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746