Material Notes:
LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food contact compliant raw materials and metal detectable.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
0.960 g/cc
0.0347 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0129 cm/cm

@Time 86400 sec
0.0129 in/in

@Time 24.0 hour
ISO 294
0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0138 cm/cm

@Time 86400 sec
0.0138 in/in

@Time 24.0 hour
ISO 294
0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
16.0 MPa
2320 psi
ISO 527
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
21.0 MPa
3050 psi
ASTM D638
Elongation at Break 38.9 %
38.9 %
ISO 527
76 %
76 %
ASTM D638
Elongation at Yield 5.6 %
5.6 %
ISO 527
7.1 %
7.1 %
ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
1 mm/min; ISO 527
1.26 GPa
183 ksi
50 mm/min; ASTM D638
Flexural Strength 24.0 MPa
3480 psi
ISO 178
27.0 MPa
3920 psi
ASTM D790
Flexural Modulus 1.18 GPa
171 ksi
ISO 178
1.27 GPa
184 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.29 J/cm
24.90 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 J
7.38 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 9.00 J
6.64 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 99.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
52.0 °C

@Thickness 3.20 mm
126 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257