J440 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Unnotched 1.18 J/cm
2.20 ft-lb/in
ASTM D256
0.539 J/cm

@Temperature -10.0 °C
1.01 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Flammability, UL94 HB
HB