ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin
Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Dat..
Flexural Modulus 1.00 GPa
145 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive app..
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Entec Hypel® PEHD32/.951 HDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Flexural Modulus 1.00 GPa

@Temperature 23.0 °C
145 ksi

@Temperature 73.4 °F
ISO 178
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer
Available in standard black.Information provided by MBA Polymers.
Flexural Modulus 1.00 GPa
145 ksi
2 mm/min; ISO 178
Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer
INNOPOL® CS 2-8302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8302 is developed for extru..
Flexural Modulus 1.00 GPa
145 ksi
conditioned, 2 mm/min; ISO 178-A
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66
PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS.
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Solvay Technyl® C 206 Nylon 6, EH50
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Techmer ES Electrafil® PP-61/EC Copolymer Polypropylene, Conductive Carbon Filled
Conductive Carbon, Powder Modified
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA..
Flexural Modulus 1.00 GPa
145 ksi
50% humidity; ISO 178
Borealis Bormed™ RD804CF Polypropylene Random Copolymer
Bormed™ RD804CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications Bormed™ RD804CF is recommended for packaging for med..
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman.
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Unipetrol PE HD LITEN® BB 75 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Unipetrol PE HD LITEN® FB 75 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Flexural Modulus 1.00 - 1.14 GPa
145 - 165 ksi
tangent; ASTM D790
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene
DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman.
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b..
Flexural Modulus 1.00 GPa
145 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene
Medium Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 2550A is a medium impact, high flow, controlled rheology copolymer of polypropylene designed for such ..
Flexural Modulus 1.00 GPa
145 ksi
cond; ISO 178
DSM Novamid® 1010C2 PA6
Easy Molding Grade
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Flexural Modulus 1.00 GPa
145 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow
Flexural Modulus 1.00 GPa
145 ksi
ASTM D 790
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer
Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l.
Flexural Modulus >= 1.00 GPa
>= 145 ksi
ISO 178
AKG Polymers Vision PP PPC TC3005 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
BASF Ultramid® S3K Balance PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Flexural Modulus 1.00 GPa
145 ksi
Spartech Spectrum® S630 MDPE Polyolefin Sheet  (discontinued **)
Data provided by the manufacturer.
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Total PPR 3260 Random Copolymer Polypropylene, Extrusion Grade
Polypropylene PPR 3260 is a random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals.
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Total Lacqrene® 9218 Polystyrene  (discontinued **)
LACQRENE® 9218 is a polystyrene modified with polyethylene. This combination gives a high level of stress crack resistance with excellent mechanical properties and good abrasion resistance. This ..
Flexural Modulus 1.00 GPa
145 ksi
Tangent; ASTM D790A
Bapolene® 3295 Polyethylene, Injection Grade
Designed to offer improved cycle times and dimensional stability This product complies with US FDA 21CFR177.1250.Applications: Food containers and closures.Bapolene® and Bapolan® are registered t..
Flexural Modulus 1.00 GPa
145 ksi
Tangent at 0.05 in/min; ASTM D790A
LyondellBasell Astryn 7523C Polypropylene Copolymer
Key Features: conventional melt flow, medium modulus polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, versatile, good processabilityApplications: autom..
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790