Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.40 GPa @Temperature 23.0 °C |
1360 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE350038 BK083 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin, developed for improved structural performance. It is also a P.. |
|||
Flexural Modulus | 9.40 GPa @Temperature 100 °C |
1360 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Flexural Modulus | 9.38 GPa | 1360 ksi | ASTM D790 |
LNP Thermocomp® LF-1006 MG Polyetheretherketone, Glass milled Glass Fiber
(discontinued **) Features: Low WarpageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still a.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 930 PET 30% Glass Reinforced Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36 PA 66 (Asia Pacific) LNP* Lubricomp* RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as Lub.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFP36S PA 66 LNP* LUBRICOMP* RFP36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Flexural Modulus | 9.37 GPa | 1360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Flexural Modulus | 9.37 GPa | 1360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66 LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA 66 LNP* THERMOCOMP* RF006S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66 LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 9.35 GPa | 1360 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ASTM D790 |
Tipco Tipcofil® AG 800 - 40% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 40% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good .. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based .. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced 15% Glass fiber reinforced and 25% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the followi.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced 40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, Conditioned Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Flexural Modulus | 9.40 GPa | 1360 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Flexural Modulus | 9.38 GPa | 1360 ksi | ASTM D790 |
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry) Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c.. |
|||
Flexural Modulus | 9.38 GPa | 1360 ksi | ASTM Value |
BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced nylon 6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times .. |
|||
Flexural Modulus | 9.37 GPa | 1360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated. |
|||
Flexural Modulus | 9.40 GPa @Temperature 23.0 °C |
1360 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Flexural Modulus | 9.41 GPa | 1360 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo.. |