Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.90 GPa | 1440 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
Nilit FRIANYL A63 W-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 1.3 mm/min; ASTM D790 |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ASTM D790 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178-93 |
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66 Description: Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Chrysler DX9 color matchedAll information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam UF0033 PPA, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam UF0033 is a Mineral Flame Retardant, Halogen Free and Red Phosphorous Free, Glass Reinforced, Polyphthalamide Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO Data |
BASF Ultramid® 1503-2 BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 1503-2 BK ND3007 is a 33% glass reinforced, heat stabilized, pigmented black injection molding PA6/6. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO Data |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Flexural Modulus | 9.90 GPa | 1440 ksi | ISO 178-93 |
Wellman Wellamid® FRGF1850-N1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |