Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.60 GPa | 1250 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 4349 Phenolic, Granular, Injection Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 7507 Phenolic, Granular, Compression Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 7507 Phenolic, Granular, Transfer Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | dry; ISO 178 |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | dry; ISO 178 |
DSM Akulon® K224-LG6 /E PA6-GF30 30% Glass Reinforced, Injection Molding, Improved UV-stability |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Adell BR-17 Nylon 6, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Adell BR-37 Nylon 6, 35% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO Data |
BASF Ultradur B 4300 G6 LS BK15073 30% Glass Filled PBT mt |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3EG6 BK00564 is a 30% glass fiber reinforced, pigmented black injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ASTM D790 |
Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced Nylon 66 designed for high strength and dimensional stability.Data provided by the manufacturer |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Flexural Modulus | 8.60 GPa | 1250 ksi | ISO 178 |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Dry) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |