| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP STAT-KON |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
| 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.100 % | 0.100 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0013 cm/cm <br>@Time 86400 sec |
0.0013 in/in <br>@Time 24.0 hour |
ISO 294 |
| 0.0010 - 0.0030 cm/cm <br>@Time 86400 sec |
0.0010 - 0.0030 in/in <br>@Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.0038 cm/cm <br>@Time 86400 sec |
0.0038 in/in <br>@Time 24.0 hour |
ISO 294 |
| 0.0030 - 0.0050 cm/cm <br>@Time 86400 sec |
0.0030 - 0.0050 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 118 MPa | 17100 psi | ASTM D638 |
| 119 MPa | 17300 psi | ISO 527 | |
| Tensile Strength, Yield | 118 MPa | 17100 psi | ASTM D638 |
| 119 MPa | 17300 psi | ISO 527 | |
| Elongation at Break | 2.4 % | 2.4 % | ASTM D638 |
| 2.4 % | 2.4 % | ISO 527 | |
| Elongation at Yield | 2.3 % | 2.3 % | ISO 527 |
| 2.4 % | 2.4 % | ASTM D638 | |
| Tensile Modulus | 9.26 GPa | 1340 ksi | 1 mm/min; ISO 527 |
| 9.65 GPa | 1400 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 144 MPa | 20900 psi | ASTM D790 |
| 181 MPa | 26300 psi | ISO 178 | |
| Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
| 8.60 GPa | 1250 ksi | ISO 178 | |
| Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 32.0 kJ/m² | 15.2 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 45.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 45.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 37.8 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
21.0 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 38.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
21.1 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 150 °C <br>@Thickness 3.20 mm |
302 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 146 °C | 295 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 147 °C <br>@Thickness 3.20 mm |
297 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 100 - 1.00e+6 ohm | 100 - 1.00e+6 ohm | ASTM D257 |