Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178 |
PolyOne Nymax™ GF 600 A 33 HS7 DX9 Black Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178 |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
North Wood Plastics PS with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Rostone Rosite® 4010ES SMC Thermoset Polyester, 22-25% Glass Reinforced
(discontinued **) Key Features: Business Machine GradeHigh strength, dimensional control, and surface smoothness.Information provided by Oneida-Rostone Group. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts .. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178 |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RVL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RVL36 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF005 PA 66 LNP* THERMOCOMP* RF005 is a compound based on Nylon 66 resin containing 25% Glass Fiber. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF006S PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006S is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PCN2615 PPE+PS (Asia Pacific) |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ISO 178-93 |
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Toyobo Vylopet® EMC430 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical pro.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Chem Polymer Chemlon 133 G Nylon 66, 33% Glass Fiber Reinforced A 33% glass fiber reinforced nylon 66 offering excellent high temperature performance, tensile strength and impact resistance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-30G Nylon 6, 30% Glass Reinforced A 30% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | dry; ISO 178 |
DSM Novamid® 3021GH30 BK629 PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu.. |
|||
Flexural Modulus | 8.30 - 15.9 GPa | 1200 - 2300 ksi | Average value: 12.2 GPa Grade Count:38 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |