Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.19 %
0.19 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
shrinkage
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.8 MPa
3310 psi
ASTM D638
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 5.50 J/cm
10.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 5VA
5VA
0.062 inch thickness
Electrical Properties Metric English Comments
Dielectric Strength 10.8 kV/mm
274 kV/in
Short Time; ASTM D149
Arc Resistance 190 sec
190 sec
ASTM D495