Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6 PA6 GR30 IM6 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | 73°F; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 202 is a two-stage, woodflour-filled phenolic molding compound formulated to provide improved impact and fatigue strength, good dimensional stability and excellent molded finish for automoti.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 L X MT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: SilverTPCI# 7210102Information provid.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Plaslube® J-4/30/TF/15 Nylon 612, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IF007 PA 6/12 (Asia Pacific) LNP* THERMOCOMP* IF007 is a compound based on Nylon 6/12 resin containing Glass Fiber. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP VF008A PA 66 LNP* THERMOCOMP* VF008A is a compound based on High Impact Nylon 66 containing 40% Glass Fiber. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight/Unspecified Filler/Reinfor.Additive: LubricantFeatures: Conductive and LubricatedAppear.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill® PA6 0685 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 8.30 GPa | 1200 ksi | ASTM D790 |
Plenco 6301 Phenolic, Granular, Injection Molded PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i.. |
|||
Flexural Modulus | 8.27 GPa @Temperature 149 °C |
1200 ksi @Temperature 300 °F |
ASTM D790 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Modulus | 8.27 GPa | 1200 ksi | ASTM D790 |
Techmer ES HiFill FR® PBT GF30 FR-S 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Non-BloomingProcessing Method: Injection MoldingInformation provided by .. |
|||
Flexural Modulus | 8.27 - 9.65 GPa | 1200 - 1400 ksi | ASTM D790 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |